Alloy 400/600 Nickel Alloy U Bend Heat Exchanger Tube Annealed Surface
Contact Person : Cherry Gao
Phone Number : +86 573 82717867
WhatsApp : +8613857354118
Minimum Order Quantity : | negotiable | Price : | 3700-9000USD/TON |
---|---|---|---|
Packaging Details : | Plywood Case / Iron Case / Bundles | Delivery Time : | 30 Days |
Payment Terms : | T / T ; L / C | Supply Ability : | 300 Tons / Month |
Place of Origin: | CHINA | Brand Name: | MTSCO |
---|---|---|---|
Certification: | ISO 9001 & PED & AD2000 | Model Number: | MTSCOHET27 |
Detail Information |
|||
Material: | 300 Series | Type: | Seamless |
---|---|---|---|
Technology: | Cold Rolled | Condition: | Soft / Hard |
Surface: | Pickling & Annealing | Length: | 6096mm |
High Light: | heat transfer tube,heat exchanger pipe |
Product Description
ASTM A269 / ASTM A213 Stainless Steel Straight Heat Exchanger Tube For Fuild And Gas
Our heat exchanger tube with pickling and annealing surface is very popular in boilers and heat exchangers industry , water heater industry , air-conditioning industry etc . This kind of seamless tubes are have a very important position in our all products .
Project | Standard | ASTM A269/A269M | ASTM A312/A312M | ASTM A213/A213M | ASTM A789/789M | ASTM A790/790M | ||||||||
Grade |
TP304 TP304L TP321 TP316 TP316L TP317 TP321 TP347 N08904/904L |
TP304 TP304L TP309S TP310S TP316 TP316L TP316Ti TP317 TP317L TP321 TP347 |
TP304 TP304L TP309S TP316 TP316L TP316Ti TP317 TP310S TP321 TP347
|
S32250 S31803 S32750 |
S32250 S31803 S32750
|
|||||||||
Size |
NPS:1/8”-48” SCH:5S,10/10S,20,30,40/40S,60,80/80S,100,120,140,160,STD,XS,XXS OD:(3.18mm-101.6mm) WT:(0.5mm-20mm) |
|||||||||||||
Length | According to customer’s request, Max. 18Meters. | |||||||||||||
Chemical composition(According to the standard) | ||||||||||||||
Eg. TP304L(ASTM)/1.4306(DIN) | ||||||||||||||
C max | Si max | Mn max | P max | S max | Cr | Ni | N max | |||||||
TP304L | 0.035 | 1.00 | 2.00 | 0.045 | 0.030 | 18.0-20.0 | 8.0-12.0 | -- | ||||||
1.4306 | 0.030 | 1.00 | 2.00 | 0.045 | 0.030 | 18.0-20.0 | 10.0-12.0 | 0.11 | ||||||
Surface Finish | Annealed, Pickled etc | |||||||||||||
Packing | Bundles/plywood cases | |||||||||||||
Applications | For fluid & gas transport; structure & machining; petrochemical; environmental protection; electricity etc | |||||||||||||
Other standards |
ASTM A270/270M ASTM B667 EN10216-5 JIS G3463 |
ASTM A213 / A213M Chemical Composition :
Elements | 304L(wt%) S30403 | 304(wt%) S30400 | 316L (wt%) S31603 | 316 (wt%) S31600 |
(C) Carbon, max | 0.035 | 0.08 | 0.035 | 0.08 |
(Mn) Manganese, max | 2 | 2 | 2 | 2 |
(P) Phosphorus, max | 0.045 | 0.045 | 0.045 | 0.045 |
(S) Sulfur, max | 0.03 | 0.03 | 0.03 | 0.03 |
(Si) Silicon, max | 1 | 1 | 1 | 1 |
(Ni) Nickel | 8.0 - 12.0 | 8.0 - 11.0 | 10.0 - 14.0 | 10.0 - 14.0 |
(Cr) Chromium | 18.0 - 20.0 | 18.0 - 20.0 | 16.0 - 18.0 | 16.0 - 18.0 |
(Mo) Molybdenum | N/A | N/A | 2.0 - 3.0 | 2.0 - 3.0 |
(Fe) Iron | Bal. | Bal. | Bal. | Bal. |
(Cu) Copper | N/A | N/A | N/A | N/A |
(N) Nitrogen | N/A | N/A | N/A | N/A |
ASTM A269 Chemical Composition :
Elements | 304L(wt%) S30403 | 304(wt%) S30400 | 316L (wt%) S31603 | 316 (wt%) S31600 |
(C) Carbon, max | 0.035 | 0.08 | 0.035 | 0.08 |
(Mn) Manganese, max | 2 | 2 | 2 | 2 |
(P) Phosphorus, max | 0.045 | 0.045 | 0.045 | 0.045 |
(S) Sulfur, max | 0.03 | 0.03 | 0.03 | 0.03 |
(Si) Silicon, max | 1 | 1 | 1 | 1 |
(Ni) Nickel | 8.0 - 12.0 | 8.0 - 11.0 | 10.0 - 14.0 | 10.0 - 14.0 |
(Cr) Chromium | 18.0 - 20.0 | 18.0 - 20.0 | 16.0 - 18.0 | 16.0 - 18.0 |
(Mo) Molybdenum | N/A | N/A | 2.0 - 3.0 | 2.0 - 3.0 |
(Fe) Iron | Bal. | Bal. | Bal. | Bal. |
(Cu) Copper | N/A | N/A | N/A | N/A |
(N) Nitrogen | N/A | N/A | N/A | N/A |
Process :
1 . We use Cold Drawn techonology to produce U bend tube
2 . U bend tubes produce will accordance to customer's drawings
3 . To avoid oxidation , inert gas (Argon) is passed through tubes ID at the required flow rate
4 . The radius is checked for its OD and wall thinning with the recommended specification
5 . We'll choose three different position or as customer's require to make sure tubes quality . We'll do physical properties and micro-structure test
6 . Visual inspection for waviness and cracks is done with Dye Penetrant Test
7 . Each tube is then hydro tested at the recommended pressure to check for leakage
Enter Your Message